Cu base wire electrode for joints and platings on Cu and Cu-alloys. Preheating is necessary for sections thicker than3 mm (100°C for each mm, 600 °max.). In case of more than 300°C preheating temperature borium containing flux addition is necessary. Preheating temperature of pure copper: 400-600°C.